Group: Forum Members
Posts: 1,
Visits: 18
|
Hello,
Been stalking these forums for a while as I am planning on making a Whitewater Kayak using Infusion.
One question I haven't been able to find the answer to, will I need to use flow media in areas where I have a contour-scrim foam core?
My layup in the Hull of the kayak will be: Mold, 2 Layers 11oz carbon, Corecell M80 6mm Contour Scrim (knife cut) Foam, 1 more layer of 11oz Carbon, Peel Ply, Vac Bag.
Do I need, or should I use a layer of flow media in-between the peel-ply and vac bag? I will definitely be using it in areas without the foam, I'm partially worried about the resin reaching the bottom layer(s) of fabric if a flow media is used.
Also, any estimation of the amount of resin that will be consumed by the foam?