Hi,

What is the best way to mark cut lines on pre-preg carbon fibre, to avoid making cuts on the mould.

Some guys at my place use white China markers but I find they aren't very precise, due to being fairly blunt.

Cheers
Steve
Reply
YouStoleMyMash
Y
Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)
Group: Forum Members
Posts: 8, Visits: 195
f1rob - 11/26/2019 9:36:08 PM
Most materials you can get a black or blue biro to show up fairly well
If you want to go the "crayon" route use verethin 
They are solid pigment not wax based like chinagraph. Gold (no99 I belive) shows up well,you can sharpen them like a normal pencil

Just got some Verithin pencils and they're working pretty well. Thanks