Is there a florescent additive for light persistence?


Author
Message
Mangy_Dog
Mangy_Dog
Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)
Group: Forum Members
Posts: 12, Visits: 45
Working on an interest led display project, in our current setup the way the multitude of leds are addressed and lit can cause some strobing. Most noticable when moving the head left to right (think the old red led display boards)

I want to try and eliminator this strobing effect by using some kind of florescent additive to clear polyurethane resin. So the florescent only needs to glow for a fraction of a second to fill in to the next led duty cycle.

Is there anything like that? I dont need to worry about colour accuracy, this is just a tungsten temperature white led...



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Mangy_Dog - 7 Years Ago
Warren (Staff) - 7 Years Ago
Steve Broad - 7 Years Ago
Mangy_Dog - 7 Years Ago
Steve Broad - 7 Years Ago
Mangy_Dog - 7 Years Ago
                         Stupid question, probably, but can't you increase the refresh rate?
Steve Broad - 7 Years Ago
Mangy_Dog - 7 Years Ago
                                 The trouble with nitpicks is they can become obsessions if you are not careful :-)
Steve Broad - 7 Years Ago
                                     Oh that happens far too often in my development stuff... :D
Mangy_Dog - 7 Years Ago
Steve Broad - 7 Years Ago