Is there a florescent additive for light persistence?


Author
Message
Steve Broad
Steve Broad
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Mangy_Dog - 12/4/2019 3:01:51 PM
Steve Broad - 12/4/2019 2:44:09 PM
Mangy_Dog - 12/4/2019 2:35:26 PM
Steve Broad - 12/4/2019 2:24:52 PM
Mangy_Dog - 12/4/2019 1:05:01 PM
Steve Broad - 12/4/2019 12:54:57 PM

You are fussy :-) If you are looking for something that lasts milliseconds then good luck and please let us know if you find anything at it would be useful :-)

Yep i am BigGrin Sorry Smile but yeah a full glow would break the refresh rate of the display... I just want to reduce strobeing... Never mind though it was only a off chance question, in case anyone knew of a pigment for it. 

Stupid question, probably, but can't you increase the refresh rate?
Its a limitation of the multiplexer... Even if it could go faster it would just mean the strobe will be slightly faster.... But it would still be there... It cant get to the rates needed for true image persistence without any artifacts.
Its also not critical tbh. it was just an off chance question that might improve it... A personal nitpick of mine BigGrin




The trouble with nitpicks is they can become obsessions if you are not careful :-)

Oh that happens far too often in my development stuff... BigGrin

Tell me about it :-) I have made a few carbon bits on my project drag car more than once, but you have to be happy with the result or it will niggle for ever.

Mangy_Dog
Mangy_Dog
Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)
Group: Forum Members
Posts: 12, Visits: 45
Steve Broad - 12/4/2019 2:44:09 PM
Mangy_Dog - 12/4/2019 2:35:26 PM
Steve Broad - 12/4/2019 2:24:52 PM
Mangy_Dog - 12/4/2019 1:05:01 PM
Steve Broad - 12/4/2019 12:54:57 PM

You are fussy :-) If you are looking for something that lasts milliseconds then good luck and please let us know if you find anything at it would be useful :-)

Yep i am BigGrin Sorry Smile but yeah a full glow would break the refresh rate of the display... I just want to reduce strobeing... Never mind though it was only a off chance question, in case anyone knew of a pigment for it. 

Stupid question, probably, but can't you increase the refresh rate?
Its a limitation of the multiplexer... Even if it could go faster it would just mean the strobe will be slightly faster.... But it would still be there... It cant get to the rates needed for true image persistence without any artifacts.
Its also not critical tbh. it was just an off chance question that might improve it... A personal nitpick of mine BigGrin




The trouble with nitpicks is they can become obsessions if you are not careful :-)

Oh that happens far too often in my development stuff... BigGrin

Steve Broad
Steve Broad
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Mangy_Dog - 12/4/2019 2:35:26 PM
Steve Broad - 12/4/2019 2:24:52 PM
Mangy_Dog - 12/4/2019 1:05:01 PM
Steve Broad - 12/4/2019 12:54:57 PM

You are fussy :-) If you are looking for something that lasts milliseconds then good luck and please let us know if you find anything at it would be useful :-)

Yep i am BigGrin Sorry Smile but yeah a full glow would break the refresh rate of the display... I just want to reduce strobeing... Never mind though it was only a off chance question, in case anyone knew of a pigment for it. 

Stupid question, probably, but can't you increase the refresh rate?
Its a limitation of the multiplexer... Even if it could go faster it would just mean the strobe will be slightly faster.... But it would still be there... It cant get to the rates needed for true image persistence without any artifacts.
Its also not critical tbh. it was just an off chance question that might improve it... A personal nitpick of mine BigGrin




The trouble with nitpicks is they can become obsessions if you are not careful :-)

Mangy_Dog
Mangy_Dog
Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)
Group: Forum Members
Posts: 12, Visits: 45
Steve Broad - 12/4/2019 2:24:52 PM
Mangy_Dog - 12/4/2019 1:05:01 PM
Steve Broad - 12/4/2019 12:54:57 PM

You are fussy :-) If you are looking for something that lasts milliseconds then good luck and please let us know if you find anything at it would be useful :-)

Yep i am BigGrin Sorry Smile but yeah a full glow would break the refresh rate of the display... I just want to reduce strobeing... Never mind though it was only a off chance question, in case anyone knew of a pigment for it. 

Stupid question, probably, but can't you increase the refresh rate?
Its a limitation of the multiplexer... Even if it could go faster it would just mean the strobe will be slightly faster.... But it would still be there... It cant get to the rates needed for true image persistence without any artifacts.
Its also not critical tbh. it was just an off chance question that might improve it... A personal nitpick of mine BigGrin




Edited 7 Years Ago by Mangy_Dog
Steve Broad
Steve Broad
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Mangy_Dog - 12/4/2019 1:05:01 PM
Steve Broad - 12/4/2019 12:54:57 PM

You are fussy :-) If you are looking for something that lasts milliseconds then good luck and please let us know if you find anything at it would be useful :-)

Yep i am BigGrin Sorry Smile but yeah a full glow would break the refresh rate of the display... I just want to reduce strobeing... Never mind though it was only a off chance question, in case anyone knew of a pigment for it. 

Stupid question, probably, but can't you increase the refresh rate?

Mangy_Dog
Mangy_Dog
Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)
Group: Forum Members
Posts: 12, Visits: 45
Steve Broad - 12/4/2019 12:54:57 PM

You are fussy :-) If you are looking for something that lasts milliseconds then good luck and please let us know if you find anything at it would be useful :-)

Yep i am BigGrin Sorry Smile but yeah a full glow would break the refresh rate of the display... I just want to reduce strobeing... Never mind though it was only a off chance question, in case anyone knew of a pigment for it. 

Steve Broad
Steve Broad
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K

You are fussy :-) If you are looking for something that lasts milliseconds then good luck and please let us know if you find anything at it would be useful :-)

Mangy_Dog
Mangy_Dog
Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)
Group: Forum Members
Posts: 12, Visits: 45
Steve Broad
Steve Broad
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I am not aware of any pigments like that.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...