mustafa
m
mustafa
posted 7 Years Ago
ANSWER
HOT
Topic Details
m
Group: Forum Members
Posts: 3,
Visits: 19
Good day,
after using GC50 , the product looks a bit foggy ,, its like this ? Or i have done some mistake in the process,
( i am using 2% catalyst from local market ). Photo no-1 is without gelcoat ,, photo no-2 is with GC50 and you can feel the deference !
please advice what to do ? Thanks.
Edited
7 Years Ago by
mustafa
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
GC-50 polyester gelcoat
mustafa
-
7 Years Ago
You do lose a little bit of clarity when using GC50, so this is quite normal and is mainly down to the fact that, even with a fairly good spraying technique, the surface that you'll be laying your...
MarkMK
-
7 Years Ago
Thank you very much your answer was very clear and helpful for me👍
mustafa
-
7 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search