MarkMK - 11/22/2019 2:42:21 PM
You do lose a little bit of clarity when using GC50, so this is quite normal and is mainly down to the fact that, even with a fairly good spraying technique, the surface that you'll be laying your fabric on will be less 'flat' on a micro level, so there will be some visual distortion

It shouldn't be sprayed too heavily, though, as this can lead to a slightly milky appearance, but you should expect a little less clarity overall when compared to parts produced with no in-mould coating

The benefits of using it, however, are worth it in many instances


Thank you very much your answer was very clear and helpful for me👍

MarkMK
MarkMK
Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
You do lose a little bit of clarity when using GC50, so this is quite normal and is mainly down to the fact that, even with a fairly good spraying technique, the surface that you'll be laying your fabric on will be less 'flat' on a micro level, so there will be some visual distortion

It shouldn't be sprayed too heavily, though, as this can lead to a slightly milky appearance, but you should expect a little less clarity overall when compared to parts produced with no in-mould coating

The benefits of using it, however, are worth it in many instances


mustafa
m
Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)
Group: Forum Members
Posts: 3, Visits: 19
Good day,
 after using GC50 , the product looks a bit foggy ,, its like this ? Or i have done some mistake in the process,
( i am using 2% catalyst from local market ).  Photo no-1 is without gelcoat ,, photo no-2 is with GC50 and you can feel the deference !
please advice what to do ? Thanks.

 

Edited 7 Years Ago by mustafa
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search