XC110 Tack Level


Author
Message
f1rob
f1rob
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
Debulk your 1st ply
If it's really bad give it a warm debulk an let it cool
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The tack does feel slightly lower than some other pre-pregs I (and others here) have used but I have not experienced the issues of it falling away from the surface after cooling.  Heating it slightly has always been enough for it to work properly on the projects I have seen done.  I wonder if your release agent is just a bit more "slippery" on the surface than others on the market?

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
KLComposites
KLComposites
Supreme Being (347 reputation)Supreme Being (347 reputation)Supreme Being (347 reputation)Supreme Being (347 reputation)Supreme Being (347 reputation)Supreme Being (347 reputation)Supreme Being (347 reputation)Supreme Being (347 reputation)Supreme Being (347 reputation)
Group: Forum Members
Posts: 26, Visits: 3.2K
Using XC110 and loving it. Very easy to get good results. Only feedback is that the tack is fairly low which can make layup a bit tricky sometimes. Warming the prepreg offers temporary relief but the material just doesn't hold and lifts away from the mold surface as soon as it cools. We're using a semi-permanent mold release available here in the States - manufactured by Axel if that means anything to anyone. Do all XC110 users think the tack is pretty low, or do we need to try a lower slip mold release?

Also, any thoughts about dying the resin system black? The only cosmetic issues we end up with sometimes is slight bridging, and the milky resin draws your eye to the flaw immediately. Changing the layup solves the problem but stuff happens and if the bridges cured black I think it would make the material a bit more idiot proof and we'd have a bit less work in the finishing process.

Thanks, all.

Nick
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search