Classicarbon
C
Classicarbon
posted 7 Years Ago
ANSWER
HOT
Topic Details
C
Group: Forum Members
Posts: 86,
Visits: 639
Do need degassing rasin always or all depend from how big item we do?
On easy composite video with the bonnet rasin wasn't degased so?
Is.always necessary?
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Degassing- Always?
Classicarbon
-
7 Years Ago
Not normally necessary, depends what you are doing. Can help with parts that have details that the fibres just cant get into, as these areas will trap bubbles. Improves the appearance of any bridged....
Hanaldo
-
7 Years Ago
I would never skip the degassing. It takes not to much time and the result will be much different.
Legoman
-
7 Years Ago
I'd agree with Hanaldo I stopped bothering with degassing ages ago and have not noticed any cosmetic difference with parts, even on the smaller ones with some detail. Quite often they will be infuse...
MarkMK
-
7 Years Ago
I am a degassing fan as well. On larger infusions I can run the resin so much faster without getting any pinholes, that it is worth it time wise. I also do a lot of closed mould work, for wich...
oekmont
-
7 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search