By Classicarbon - 8/22/2019 6:41:14 AM
Do need degassing rasin always or all depend from how big item we do? On easy composite video with the bonnet rasin wasn't degased so? Is.always necessary?
|
By oekmont - 9/2/2019 6:33:24 AM
I am a degassing fan as well. On larger infusions I can run the resin so much faster without getting any pinholes, that it is worth it time wise. I also do a lot of closed mould work, for wich degassing is necessary in my opinion. However, i have to admit that easier parts can be done without degassing. But as I do it for living, I love the extra insurance to always get perfect parts. One tiny pinhole and you have to clearcoat the whole part to get a perfect finish.
|
|