Argo
Argo
posted 7 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 14
Hi there
I like the concept of low-temperature pre-pregs but living in New Zealand am thinking shipping would be problematic, given the requirement of keeping the material frozen.
Recently I came across articles describing UV curable pre-preg. This would eliminate (I imagine) any shipping problems and potentially make curing even simpler than low temp pre-preg. Has Easy Composites carried out any research on this material? Apologies if this has already been talked about, I did do a search before posting
Cheers.
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
UV cure pre-preg
Argo
-
7 Years Ago
If you are referring to the X-Preg system as low temp curing, then it really isn't, it is more of a medium temp cure. Shipping shouldn't be any issue as the material as an out-life of one month, and ...
Hanaldo
-
7 Years Ago
Hi Hanaldo Thanks for this advice, great to know. I didn't realise the X-Preg system had such a resilient shelf-life. I guess in my case, just so long as the shipment doesn't sit for too long on a ho...
Argo
-
7 Years Ago
If it's any comfort, I'm in Perth Australia and I've bought many metres of X-Preg from Easy Composites, as well as Easy Preg before that. I've never had any issues, so even though you're a it further...
Hanaldo
-
7 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search