By Argo - 8/18/2019 1:24:32 AM
Hi there
I like the concept of low-temperature pre-pregs but living in New Zealand am thinking shipping would be problematic, given the requirement of keeping the material frozen.
Recently I came across articles describing UV curable pre-preg. This would eliminate (I imagine) any shipping problems and potentially make curing even simpler than low temp pre-preg. Has Easy Composites carried out any research on this material? Apologies if this has already been talked about, I did do a search before posting 
Cheers.
|
By Hanaldo - 8/21/2019 10:41:32 AM
If it's any comfort, I'm in Perth Australia and I've bought many metres of X-Preg from Easy Composites, as well as Easy Preg before that. I've never had any issues, so even though you're a it further, I think you should be fine
|
|