It depends on the plastic.  Uni-Mould uses styrene based plastics so anything styrene based can be dissolved or surface attacked.  eg polystyrene.   The epoxy is much more inert and does not effect virtually any plastics. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Kevin254
K
Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)
Group: Forum Members
Posts: 4, Visits: 15
Greetings,

I have a few patterns that are made from either plastic or glass. I wanted to know if the above gelcoat systems would effectively work on the materials listed. Are there plastics that are incompatible with either of the gelcoat systems?
Thanks.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search