			            It depends on the plastic.  Uni-Mould uses styrene based plastics so anything styrene based can be dissolved or surface attacked.  eg polystyrene.   The epoxy is much more inert and does not effect virtually any plastics.                 
			            
  				
			            Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant                     
                     
                                            
                         
                    
                  
             |