By Kevin254 - 6/16/2019 11:23:51 AM				
            
                      
            Greetings,
  I have a few patterns that are made from either plastic or glass. I wanted to know if the above gelcoat systems would effectively work on the materials listed. Are there plastics that are incompatible with either of the gelcoat systems? Thanks. 
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By Warren (Staff) - 6/25/2019 9:20:02 AM				
            
                      
            It depends on the plastic.  Uni-Mould uses styrene based plastics so anything styrene based can be dissolved or surface attacked.  eg polystyrene.   The epoxy is much more inert and does not effect virtually any plastics. 
           
		 | 			
		 
	
	
						
		 	
		
	 |