Hello,
I want to make tubes from prepreg. I will use shrink tape for consolidation. unfortunately I can not control the ramping of my oven. I can only adjust it to a certain temperature. 
Is it possible to pre-heat the oven up to curing temperature ( for example 100 degree Celsius) and then put the parts inside ?
tnx