Removing a hair from cured resin


Author
Message
Bhamoggy
B
Supreme Being (290 reputation)Supreme Being (290 reputation)Supreme Being (290 reputation)Supreme Being (290 reputation)Supreme Being (290 reputation)Supreme Being (290 reputation)Supreme Being (290 reputation)Supreme Being (290 reputation)Supreme Being (290 reputation)
Group: Forum Members
Posts: 38, Visits: 420
Anyone got any tips how to remove a fine hair from cured resin?
It’s a largish table with glasscast 50 and a flood coat of glasscast 3.
I don’t want to sand the whole table down and do another pour over the top just for a small hair.
There must be something I can try instead?