Removing a hair from cured resin

http://www.talkcomposites.com/Topic32663.aspx

By Bhamoggy - 4/19/2019 10:05:00 PM

Anyone got any tips how to remove a fine hair from cured resin?
It’s a largish table with glasscast 50 and a flood coat of glasscast 3.
I don’t want to sand the whole table down and do another pour over the top just for a small hair.
There must be something I can try instead?
By JasonFL - 4/20/2019 12:55:14 PM

Grind the hair out, mask that section off, re pour. Wet sand then polish. It should match up perfect if your polishing skill is up to task.