Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Removing a hair from cured resin
Removing a hair from cured resin
Post Reply
Like
4
Removing a hair from cured resin
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
JasonFL
JasonFL
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 51,
Visits: 707
Grind the hair out, mask that section off, re pour. Wet sand then polish. It should match up perfect if your polishing skill is up to task.
Jason
Reply
Like
3
Bhamoggy
B
Bhamoggy
posted 7 Years Ago
ANSWER
HOT
Topic Details
B
Group: Forum Members
Posts: 38,
Visits: 420
Anyone got any tips how to remove a fine hair from cured resin?
It’s a largish table with glasscast 50 and a flood coat of glasscast 3.
I don’t want to sand the whole table down and do another pour over the top just for a small hair.
There must be something I can try instead?
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search