Anyone got any tips how to remove a fine hair from cured resin?
It’s a largish table with glasscast 50 and a flood coat of glasscast 3.
I don’t want to sand the whole table down and do another pour over the top just for a small hair.
There must be something I can try instead?
JasonFL
JasonFL
Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)
Group: Forum Members
Posts: 51, Visits: 707
Grind the hair out, mask that section off, re pour. Wet sand then polish. It should match up perfect if your polishing skill is up to task.

Jason
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search