Cutting carbon fiber plate with perfect results


Author
Message
S_Carbon_fibre
S
Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)
Group: Forum Members
Posts: 17, Visits: 89
oekmont - 2/22/2019 8:26:29 PM
yes, these are exactly the disc dimension I use. I guess the machine will work too. I am using one where the motor slides on a rail above, so the carbon plate can't get scratched from sliding on a metal surface. You may have to improvise to mount the disc. I used a small ring of a worn down angle grinder disc as a chim, otherwise the disc would have been too narrow.

Thanks for the response! I will give it a try. it seems the ones that the motor slides are quite expensive so I think I will go for one similar to the link I sent above..

oekmont
oekmont
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
yes, these are exactly the disc dimension I use. I guess the machine will work too. I am using one where the motor slides on a rail above, so the carbon plate can't get scratched from sliding on a metal surface. You may have to improvise to mount the disc. I used a small ring of a worn down angle grinder disc as a chim, otherwise the disc would have been too narrow.

S_Carbon_fibre
S
Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)
Group: Forum Members
Posts: 17, Visits: 89
oekmont - 2/22/2019 1:48:17 PM
An electric tile cutter. Optimal would be a cutting disc (narrow) from a big angle grinder because the diamond discs quickly wear down and become blunt when cutting cf. This is my setup for straight plate cutting.

thanks for the response! It sounds good, I would like to give it a try. Would something like this work for example?
https://www.amazon.de/dp/B00E98C6ZQ/ref=sspa_dk_detail_0?psc=1&pd_rd_i=B00E98C6ZQ&pd_rd_w=ttKCE&pf_rd_p=00903874-3af0-47e0-8622-ee58087f71cf&pd_rd_wg=E4JJ5&pf_rd_r=BWKFTZXQ3Z6KDPZRCQMT&pd_rd_r=17dd53b3-36d7-11e9-96c1-8d8439bbf4e3
or you mean a handheld one?

Also, would you recommend a disc like this one?
https://www.amazon.de/Olbrich-Industriebedarf-Trennscheibe-180x1-Edelstahl-Metall/dp/B01BWMXGDM/ref=sr_1_1?ie=UTF8&qid=1550864206&sr=8-1&keywords=cutting+disc+180mm

Thanks!

Edited 7 Years Ago by S_Carbon_fibre
oekmont
oekmont
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
An electric tile cutter. Optimal would be a cutting disc (narrow) from a big angle grinder because the diamond discs quickly wear down and become blunt when cutting cf. This is my setup for straight plate cutting.

S_Carbon_fibre
S
Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)Supreme Being (154 reputation)
Group: Forum Members
Posts: 17, Visits: 89
Hello,

I know this topic has been discussed here before. I am looking for a solution to cut carbon fiber sheets. So far I got perfect results only outsourcing to a water-jet cutter but it is expensive to use on a regular basis. I tried driving a dremel with different discs (diamond and for plastic PVC) on a linear  guide, the result is great but not perfect. There is still a little bit of burr left on the edge or I guess the resin coating is slightly burnt.. it is hard to tell but it is not perfect. Any hints or ideas ?