Darren
Darren
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 54,
Visits: 916
I decided to bite the bullet and infuse the part.
Found to tiny leaks in the actual bagging film, sealed them off with some bagging tape and all worked out ok.
Reply
Like
2
Matthieu Libeert
Matthieu Libeert
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
you have chances to get leaks,
But I think its all a matter of how you work on your mould...
If you use all the steps; gelcoat, coupling coat, tooling resin (4 layers) the chances are minimal!
make sure you have no airpockets in your tooling resin coats by using a roller and tighten all the corners firmly against your part while making the mould.
If you want to be fully sure; I sand the back of the mould once cured, removing all sharp edges and coat it again with a thick layer of resin.
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
scottracing
scottracing
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
Have you done a drop test with a vac gauge? Just bag up the mould without any material and see if theres a vac drop, id it a 1 piece mould or has it several parts / joins?
Reply
Like
3
Darren
Darren
posted 7 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 54,
Visits: 916
Whats the chances of a uni mould being porous?
Im on my second attempt at trying to get a leak free bag on this car hatch back but still no luck.
I feel I'm no amateur at the bagging process but not having much joy with this one.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search