Porous mould?

http://www.talkcomposites.com/Topic31458.aspx

By Darren - 12/30/2018 6:21:25 PM

Whats the chances of a uni mould being porous? 

Im on my second attempt at trying to get a leak free bag on this car hatch back but still no luck.
I feel I'm no amateur at the bagging process but not having much joy with this one.
By Darren - 12/31/2018 4:24:46 PM

I decided to bite the bullet and infuse the part.
Found to tiny leaks in the actual bagging film, sealed them off with some bagging tape and all worked out ok.