aluminium plate is not adhering to a carbon fiber laminate.Is it because my aluminium surface is too smooth?
I tried etching process to make it rough.But It did not work out well.Is sanding a better option than etching?
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Singhnishesh - 8 Years Ago
scottracing - 8 Years Ago
Singhnishesh - 8 Years Ago
matthieutje65 - 8 Years Ago
f1rob - 8 Years Ago
Singhnishesh - 8 Years Ago
Singhnishesh - 8 Years Ago
matthieutje65 - 8 Years Ago
f1rob - 8 Years Ago
Singhnishesh - 8 Years Ago
Zorbit - 7 Years Ago
Singhnishesh - 8 Years Ago
f1rob - 8 Years Ago
     Thank you
Singhnishesh - 8 Years Ago
Singhnishesh - 8 Years Ago
f1rob - 8 Years Ago
Singhnishesh - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search