aluminium plate is not adhering to a carbon fiber laminate.Is it because my aluminium surface is too smooth?
I tried etching process to make it rough.But It did not work out well.Is sanding a better option than etching?
Reply
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
Sanding will be fine
80grits perfect,just blow down,decrease an bond
If you really want a good bond drill a couple of holes an rivet the part on as you glue it
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Singhnishesh - 7 Years Ago
scottracing - 7 Years Ago
Singhnishesh - 7 Years Ago
matthieutje65 - 7 Years Ago
f1rob - 7 Years Ago
Singhnishesh - 7 Years Ago
Singhnishesh - 7 Years Ago
matthieutje65 - 7 Years Ago
f1rob - 7 Years Ago
Singhnishesh - 7 Years Ago
Zorbit - 6 Years Ago
Singhnishesh - 7 Years Ago
f1rob - 7 Years Ago
     Thank you
Singhnishesh - 7 Years Ago
Singhnishesh - 7 Years Ago
f1rob - 7 Years Ago
Singhnishesh - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search