Hi I did a pour a couple of days ago with glass cast 3 on some sealed wood and went over it after 10 minutes with a heat gun to help get rid of the bubbles but I’m guessing some more came up over night and now there in the set resin. Is there anyway of getting rid of them after it’s set or are they there for good now?