Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Sounds like perhaps slightly more resin needed in the sealing coat to ensure it was fully sealed.
If the bubbles are close to the surface, you can usually sand them out then fill them in. If there are quite a few, it is generally quicker to fill them in then do another flood coat over the whole project rather than sand level and polish the whole project after the repairs.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|