I have just finished my first epoxy coffee table and i sanded and polished it as per the video but it is coming up to a satin finish at best not a high gloss. what am i doing wrong?

Thanks in advance
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
myakpaul - 7 Years Ago
Bhamoggy - 7 Years Ago
myakpaul - 7 Years Ago
Bhamoggy - 7 Years Ago
                     https://ibb.co/igKxwL https://ibb.co/cCqRqf
Bhamoggy - 7 Years Ago
myakpaul - 7 Years Ago
Bhamoggy - 7 Years Ago
Warren (Staff) - 7 Years Ago
myakpaul - 7 Years Ago
Warren (Staff) - 7 Years Ago
Bhamoggy - 7 Years Ago
Bhamoggy - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search