japcarmaniac
japcarmaniac
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 53,
Visits: 157
is it realy a nightmare to cut black diolen? it looks like a good material to practice with but if it cant be trimmed to an acceptable standard its usless for making parts that look like carbon but without the need for carbons properties.
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
diolen??
japcarmaniac
-
13 Years Ago
I did not try to cut it with a good pair of household scissors, but I think a new good quality pair...
Joe
-
13 Years Ago
sorry i meant after it had cured. thanks
japcarmaniac
-
13 Years Ago
Diolen can go 'fluffy' on the trimmed edge, this is more of a problem with wet layup as the cores of...
Paul (Staff)
-
13 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search