Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)
Group: Administrators
Posts: 134, Visits: 614
Diolen can go 'fluffy' on the trimmed edge, this is more of a problem with wet layup as the cores of the fibre may not be fully wetted out, with infusion it shouldn't be a problem. it's fairly easy to clean up anyway with some 400grit sand-paper.

Paul Statham
Easy Composites / Carbon Mods - Technical
japcarmaniac
japcarmaniac
Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)
Group: Forum Members
Posts: 53, Visits: 157
sorry i meant after it had cured.

thanks


Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
I did not try to cut it with a good pair of household scissors, but I think a new good quality pair should do the trick.

However, Diolen will cut easily with decent composite scissors.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
japcarmaniac
japcarmaniac
Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)
Group: Forum Members
Posts: 53, Visits: 157
is it realy a nightmare to cut black diolen? it looks like a good material to practice with but if it cant be trimmed to an acceptable standard its usless for making parts that look like carbon but without the need for carbons properties. 