Hi Team.
Im using XC110 and looking for the clear film as the top coat to increase it's thickness,
But I did not see it on easycomposite,please help to advise .

Thanks
Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
dinh gia truyen - 9/18/2018 5:55:25 AM
Hi Team.
Im using XC110 and looking for the clear film as the top coat to increase it's thickness,
But I did not see it on easycomposite,please help to advise .

Thanks


XC110 if cured and used properly does not need an additional layer of resin on the surface to get a good cosmetic result.  The XA130 film adhesive we do sell is designed for making honeycomb and cored sheet.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Steve Broad
Steve Broad
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Why do you want to increase its thickness? Why not simply use a heavier cloth?
Hanaldo
Hanaldo
Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I feel like he is wanting a clear coat to increase the 'depth' of the finish rather than the 'thickness' of the part???
oekmont
oekmont
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
Maybe a clear inmould coating could fulfil  your needs.

dinh gia truyen
dinh gia truyen
Supreme Being (136 reputation)Supreme Being (136 reputation)Supreme Being (136 reputation)Supreme Being (136 reputation)Supreme Being (136 reputation)Supreme Being (136 reputation)Supreme Being (136 reputation)Supreme Being (136 reputation)Supreme Being (136 reputation)
Group: Forum Members
Posts: 6, Visits: 34
Hanaldo - 9/19/2018 2:19:41 PM
I feel like he is wanting a clear coat to increase the 'depth' of the finish rather than the 'thickness' of the part???

Yes, it is correct.
Thank you.

Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
It would unlikely work very well.  For a start the adhesive film is supported by a thin glass netting which would "haze" the look of the carbon fibre.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search