Kayak polo paddle repair


Author
Message
javier
javier
Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)
Group: Forum Members
Posts: 7, Visits: 36
HÍ'm writing from Spain.

I need some help to fix up a Kayak Polp paddel. Ih has a yellow band surrounding it all that it's suposed to be a Kevlar textil band fixed with epoxi.

I've found the Video "How to Repair a Damaged Composite Canoe or Kayak" and I thought I may find help here Wink

Could you please help me with the right choice of the materiarls I may need?

 

Thank you very much.

 

Javier
Replies
javier
javier
Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)
Group: Forum Members
Posts: 7, Visits: 36
Great!

I really appreciate your help!

Having a look at the shop, there's something I'm not sure of. For example at the flat braid, the title says "Lightweight Kevlar Flat Braid 300g 32mm"  and then it says "Quantity"

How much may I need to repair both blades....

Thank you very much

Javier
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Quantity is the length in metres that you want. I would think either 1m or 2m would be fine. Just measure the circumference of the blade edge and multiply it by 2 (for both blades).

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
javier
javier
Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)Supreme Being (85 reputation)
Group: Forum Members
Posts: 7, Visits: 36
Let's go!!

Thank you.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
javier - 14 Years Ago
Matt (Staff) - 14 Years Ago
Matt (Staff) - 14 Years Ago
javier - 14 Years Ago
Matt (Staff) - 14 Years Ago
javier - 14 Years Ago
javier - 14 Years Ago
Matt (Staff) - 14 Years Ago
                 Let's go!! Thank you.
javier - 14 Years Ago