Hi,
I did my first test piece (900 x 300 mm MDF) with Glasscraft 3 and getting some waves and pits.
Can you please advise what is the ‘work time’ for this product, I have looked at the spec sheets but does not offer this info only ‘curing time’ @ 25 deg.
So what I am looking for is - the time duration after mix I can use the heat gun. I have looked at various videos on You Tube re ‘waves’ and ‘pits’ and I am thinking the reason for my waves result is using the heat gun after the ‘work time’ (a term used in several of the videos).

The ‘pitting’ I am not sure what is causing that.

I am new to resin art so working with epoxy is a learning curve for me and I am determined to get the glass finish I see everyone else achieving although I am acutely aware that epoxy can be rather sensitive and a lot of precautions to be taken that as a newbie is very important to me.

Thank you for your input / response and have a lovely weekend.