EF80 / EL2 hybrid part advice please


Author
Message
FLD
FLD
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Thanks for the reply.  I might play safe and use a peel ply to give a good bonding surface with an aim for a full cure.  Should prove interesting.
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi,

It's a good question but yes it should be possible to bond EL2 to EF80 and then subsequently EF80 to EL2, particularly if you laminate the EL2 onto the EF80 when the EF80 has cured to its B stage and then again the EF80 onto the EL2 whilst that is at its B stage. However, and I don't often say this, we haven't tested this so it would be new ground and I would suggest doing a small test 'token' area first to establish that this works as you want/need it to and also to confirm that the strength of the bond and the behavior of the finished componant would be as you want it.

If at either stage you don't catch the last resin during its 'firm but still tacky' B-stage then you will need to cure it off fully, then heavily key the surface to ensure a mechanical bond.

I hope this helps and look forward to seeing how this interesting project goes.

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
FLD
FLD
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I'm looking at making a front airdam for my car but its pretty low.  Chances are I'll catch it!  EF80 looks ideal for my flexibility needs!  The downside is that I'd need some rigidity in the mounting so it doesn't just rip off.  My thought is to use EF80 for the front 'at risk' part and EL2 in the main mounting panel.  If I lay a partial thickness in EF80 and let it cure followed by an EL2 layer in just the mounting panel then a final EF80 layer will the layers bond correctly?

My other option would be some large penny washers set into the EF80 to stop it being ripped off.  Would this be a better approach?