What went wrong ???


Author
Message
SebRS
SebRS
Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)
Group: Forum Members
Posts: 29, Visits: 558
I agree this error.

And with my own experience, i can advice you to apply 2 coats of tooling Gel coat, as the first one looks too thin in the angles

You final part looks like there is not enough resin? or maybe some leaks?

Regards,

Seb.
Edited 13 Years Ago by SebRS
mickthecat
mickthecat
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 4, Visits: 32
Thanks guys.

I basically followed the video tutorial to the letter. Had no problems making the mould. The finished part was pretty much stuck fast to the mould & has pulled the dried resin off the part & is also stuck the mould itself. I put plenty of PVA on prior to the resin & stuck to the recommended drying times etc  Sad

Ahh well.......back to the drawing board

Cheers

Mick
neilb
neilb
Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)
Group: Forum Members
Posts: 107, Visits: 504
from the photo's i can only see 1 error and that is in pic 2 at the top left of the piece, the hole needs to be filled with plastercene or wax to stop a 'mechanical lock', as for the finished cf piece, as previously asked a little more info would be helpfull.
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
could you give us a bit more information on how you did everything in more detail? maybe we can find THE error or some errors Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




mickthecat
mickthecat
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 4, Visits: 32
I thought I'd covered all bases, studied the tutorial videos & took my time but........................its all gone horribly wrong Crying

What have I done wrong ?

Thanks,  Mick
Attachments
photo 1[1].JPG (204 views, 60.00 KB)
photo 2[1].JPG (205 views, 83.00 KB)
photo 3[1].JPG (207 views, 94.00 KB)
photo 4[1].JPG (212 views, 115.00 KB)
GO