By mickthecat - 9/6/2012 7:28:44 PM

I thought I'd covered all bases, studied the tutorial videos & took my time but........................its all gone horribly wrong Crying

What have I done wrong ?

Thanks,  Mick
By SebRS - 9/7/2012 1:05:41 PM

I agree this error.

And with my own experience, i can advice you to apply 2 coats of tooling Gel coat, as the first one looks too thin in the angles

You final part looks like there is not enough resin? or maybe some leaks?