Epoxy resin infusion in a glassfiber/polyester mould?
Epoxy resin infusion in a glassfiber/polyester mould?
Post Reply
Like
3
Epoxy resin infusion in a glassfiber/polyester mould?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Sjogren-Racing
Sjogren-Racing
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 59
Hello
I´m gonna buy your infusionkit with epxy for making a roofpanel in carbon.
My problem is that my mold is in fiberglass and polyester.
What i have read is that not so good for use with epoxy? I read that the only soloution is to have PVA that isolate the polyester from the epxyresin?
But if i use
https://www.easycomposites.co.uk/clearpol-iso-npg-clear-polyester-gelcoat
should that work? Becouse its a polyester gelcoat that work with epoxy.
I am thinking wrong? Or is that gonna work?
I am from Sweden so sorry if i spell wrong.
Best regards Magnus
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Epoxy resin infusion in a glassfiber/polyester mould?
Sjogren-Racing
-
13 Years Ago
Should work I guess, epoxy bonds well on polyester but polyester doesn't on epoxy. This means your...
matthieutje65
-
13 Years Ago
Thanks for your answer:) I have think the same way as you. But i need a 100% answer. Can i apply...
Sjogren-Racing
-
13 Years Ago
I have no experience in spraying gelcoat, always brush it on, but a gelcoat spraygun is next on my...
matthieutje65
-
13 Years Ago
[quote][b]Sjogren-Racing (02/09/2012)[/b][hr]Thanks for your answer:) I have think the same way as...
fgayford
-
13 Years Ago
Hi, I had good luck spraying GC50 with a 3.9mm tip on a G100 spraygun. Maybe you can spray...
Joe
-
13 Years Ago
I got a answer to my first question by mail yesterday. I copy it here so everyone can see: " Yes,...
Sjogren-Racing
-
13 Years Ago
So better to use wax first then pva? I ask because I have the same issue. I inherited a polyester...
mikew
-
13 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search