By mikew - 11/18/2012 11:39:45 AM				
            
                      
            So better to use wax first then pva?
  I ask because I have the same issue. I inherited a polyester mould and wiped it with 2 coats of pva.  Did the (epoxy) infusion last night and it was VERY hard to release the part.  I don't want to use the GC50, I don't think there is any need.
           
		 |