The way I understand it the perforated film and the mesh has the same function, exept that the film allows excess resin to flow back up to a soaker, is this correct? Is that a better method than mesh without soaker?
If film and soaker is used, does that remove the need for the mesh? Does the film allow the same amount of flow during the infusion?

Also, i was going for the Epoxy Tooling Gel Coat and the Epoxy Mould Making Putty, but I´m now thinking of going with the Uni-Mould system, could somebody explain what the practical difference is?



/Cheers from a still snowy sweden.
Edited 13 Years Ago by Zekewarg
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search