The way I understand it the perforated film and the mesh has the same function, exept that the film allows excess resin to flow back up to a soaker, is this correct? Is that a better method than mesh without soaker?
If film and soaker is used, does that remove the need for the mesh? Does the film allow the same amount of flow during the infusion?

Also, i was going for the Epoxy Tooling Gel Coat and the Epoxy Mould Making Putty, but I´m now thinking of going with the Uni-Mould system, could somebody explain what the practical difference is?



/Cheers from a still snowy sweden.
Edited 13 Years Ago by Zekewarg
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Hi,

The perforated release film is more used in vacuum wet laid composites. You wet your fabric in your mold with a brush or roller or whatever. Then you put your perforated film, then breather (that will soak excess resin thru the holes of the perforated film), then vacuum it all with your pump. Controlling the amount of vacuum in your mold will make you able to tune resin to fabric ratio. If you want to do so, always use the same amount of breather, and same film material and of course same amount of fabric. That way, the only thing that will change is the vacuum level. Weighting the fabric before processing and the part after its cured will let you know how much resin you have at the end. More vacuum will squeeze more resin out of the laminate. In general, people are looking to have 60% fabric and 40% resin. More resin will lead to heavier and weaker composite etc, less resin may lead to pinholes etc. 

The infusion mesh is intended to be used in... infusion process. You lay your fabric in your mold, then you put peel ply, then the mesh, then vacuum bag. You pull vacuum with your pump, and then you can inject/pull your resin inside it all.

So, these are two different things. Then you need to decide which way you wanna build your parts: wet lay and vacuumed, or vacuum infusion (pulling the resin in last place once all is vacuumed).

 



 


    A $1000 electronic device will always protect a 10 cents fuse
Edited 13 Years Ago by Joe
Zekewarg
Zekewarg
Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)
Group: Forum Members
Posts: 42, Visits: 241
Thanks to Joe, great advice as always!
My initial plan was to just use wet lay since i thought that infusion would be time consuming.
But after thinking about it and reading a lot I`m gonna go with infusion, at least for my bigger project and all projects that require high structural
strenght. I just now bought a big batch of everything i´ll need for wet lay, probably best to learn that first, then transition to infusion.

Any thoughts on Uni-Mold vs. Gel coat and Putty?
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
I've just uploaded a sneak-peak video of the Uni-Mould system for forum members only. If you'd like to get a better idea of it (sorry, it's a LONG video) then you can see an early edit of part 1 of our new series here: http://www.talkcomposites.com/264/Sneak-Preview-Video--Using-Uni-Mould-to-Make-a-Mould-for-a-Car-Bonnet--Comments-Welcome?Keywords=Perforated%20film%20and/%20%20mesh?

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Zekewarg
Zekewarg
Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)
Group: Forum Members
Posts: 42, Visits: 241
Brilliant Matt!

Thanks a lot, now it makes sense. And Uni-mould seems to be the right choice for me.
Which is great since a couldn´t wait and already ordered it. Smile
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Zekewarg (26/01/2012)
Brilliant Matt!

Thanks a lot, now it makes sense. And Uni-mould seems to be the right choice for me.Which is great since a couldn´t wait and already ordered it. Smile
Héhé... Reminds me someone i know very well Whistling

Good luck with ur project, and dont forget the pics Wink

 



 


    A $1000 electronic device will always protect a 10 cents fuse
Zekewarg
Zekewarg
Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)
Group: Forum Members
Posts: 42, Visits: 241
I´ll make sure to post pics as soon as I get the first finished cast.
The stuff should be here monday or tuesday and I´ll dig right into it.
10 minutes after that I will probably be screaming for help.
japcarmaniac
japcarmaniac
Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)
Group: Forum Members
Posts: 53, Visits: 157
seen the vid.....excellent stuff!!! cant wait to see a part made from it.


Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Cool video.... i wish I was a hacker i would sneak thru your computer and see the rest hahaha. Teasers are always a problem to me, I never have enough, especially when good quality is involved.

Very professional as always.

Cheers from Belgium.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search