turner mum
t
turner mum
posted 8 Years Ago
ANSWER
HOT
Topic Details
t
Group: Forum Members
Posts: 2,
Visits: 3
Hi
I have made a mosaic using Mod Podge glue over card and paper and want to now use glass cast over it. Will they react badly together? Or is mod podge a suitable surface to take glass cast?
Many thanks
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
GlassCast3 surface suitability
turner mum
-
8 Years Ago
Hi, We don't see any problem with coating epoxy over the mod podge. Similar projects are done with PVA glue with no problem. In fact for your project, you want to ensure you get a good coating of th...
Warren (Staff)
-
8 Years Ago
One more quick question: on many of the youtube videos I have watched using various different resins, they have used a blowtorch to remove air bubbles. Your website says that this is not necessary. I...
turner mum
-
8 Years Ago
In 99% of cases you won't need to use one, however it can be a nice safety net to have one available or a heat gun. Leave the resin 10-15minutes after you have poured and leveled it and you should...
Warren (Staff)
-
8 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search