In 99% of cases you won't need to use one, however it can be a nice safety net to have one available or a heat gun. Leave the resin 10-15minutes after you have poured and leveled it and you should find the bubbles have self degassed.  Any stubborn bubbles can be given the blow torch treatment.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
turner mum
t
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 2, Visits: 3
One more quick question: on many of the youtube videos I have watched using various different resins, they have used a blowtorch to remove air bubbles. Your website says that this is not necessary. Is it worth me having such a tool ready just in case of bubbles forming, or does your product really rid itself of air bubbles as it cures?

Many thanks
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Hi,

We don't see any problem with coating epoxy over the mod podge.  Similar projects are done with PVA glue  with no problem.   In fact for your project, you want to ensure you get a good coating of the mod podge to seal in the  card and paper.  This is because, lower grade cards and paper  have a tendency to soak up liquid  and go translucent - imagine wet newspaper.  So a sealing coat of mod podge or PVA glue  will protect the paper from the resin soaking in and thus you can maintain  the original  finish.   If you have some spares knocking around, i might be a good idea to knock up a test piece to experiment with mod podge and the resin so you get the right amount of coverage without the resin soaking in.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
turner mum
t
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 2, Visits: 3
Hi

I have made a mosaic using Mod Podge glue over card and paper and want to now use glass cast over it. Will they react badly together? Or is mod podge a suitable surface to take glass cast?

Many thanks

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search