Prepreg for infusion


Author
Message
Carbonphoenix
Carbonphoenix
Supreme Being (165 reputation)Supreme Being (165 reputation)Supreme Being (165 reputation)Supreme Being (165 reputation)Supreme Being (165 reputation)Supreme Being (165 reputation)Supreme Being (165 reputation)Supreme Being (165 reputation)Supreme Being (165 reputation)
Group: Forum Members
Posts: 12, Visits: 134
Hey all.

I love the prepreg fabric, as I can get it cut very neatly, and concentrat on weave pattern directions, and find it all very clean.
However, I am struggling to have a have a non pin hole / dry finish.
So I am contemplating putting a layer of resin down before sticking the prepreg into place and maybe usng it in this manner and go infusing (hence why posted here )

Anyone tried this?