Best way to get flat gloss finish


Author
Message
duke
duke
Supreme Being (117 reputation)Supreme Being (117 reputation)Supreme Being (117 reputation)Supreme Being (117 reputation)Supreme Being (117 reputation)Supreme Being (117 reputation)Supreme Being (117 reputation)Supreme Being (117 reputation)Supreme Being (117 reputation)
Group: Forum Members
Posts: 10, Visits: 114
I have several infused parts that have run dry in the mold with a non flat finish on the mold side. What's the best way of fixing this? It seems too uneven to solve with clear coat unless Iay down a looot of layers?