Another thing to consider if the shape is quite rough, is maybe making a "splash" mould to use to make a rigid pattern which you can then sand shape and modify to perfection before taking the final production mould from it.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Sort of depends what kind of rubber it is. If it's a silicone (unlikely but possible), then you don't need to do much to it (but you will have trouble with getting the gel coat to form a nice surface on it!). If it is a natural rubber or a polyurethane elastomer (most likely), then you will need to use a release agent. For a natural rubber, PVA would be required to prevent the gelcoat from reacting with. For a polyurethane, standard release wax would do, or something like Stoner Rapid Release/Mann Ease 200.
aliwes
a
Supreme Being (197 reputation)Supreme Being (197 reputation)Supreme Being (197 reputation)Supreme Being (197 reputation)Supreme Being (197 reputation)Supreme Being (197 reputation)Supreme Being (197 reputation)Supreme Being (197 reputation)Supreme Being (197 reputation)
Group: Forum Members
Posts: 7, Visits: 17
Evening all,

I want to make some carbon light blocks to mount my car's rear lights to. The current setup is a wedge made from what appears to be rubber - very flexible with a textured surface.

my question is; How do I prepare the wedge for making the mould using the uni-mould system?

Any tips gratefully received.

Thanks in advance.

Al
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search