Hello!
I can't find answer of this question. This is about making a RC Airplanes fuselage. All composite fuselages are making by hand layup. My fuselage for example weight afer demold is about 550gr. There is 50g glass cloth outside/1.5mm herex/50g glass cloth inside sandwich. And of course some carbon reinforcements. The question is - IS it possible to make fuselage like this in resin infusion in this weight?