Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Are you using a polyester or vinyl ester resin? It looks like a high degree of shrinkage to me. If youre using poly or vinyl then this is pretty normal in my experience. If you're using epoxy then its a bit odd and I suspect you demoulded too soon. Print through of the Soric is quite normal if your laminate is thin on either side, but this looks a bit worse than that.
No harm in having the Soric edges exposed, purely a cosmetic choice not to.
|