Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
If you have that much air entrapped then maybe the temperature was too low and/or you were too aggressive with the mixing. We would not normally expect that many pinholes. Have you got some photos showing the issue?
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|