Tight corners without spray tack?


Author
Message
carbon man
carbon man
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
Hi can I have some tips on how to get carbon to sit in tight and straight without using spray glue? 
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You can use tape on the fabric edge to help a bit, but without any spray tack, you are reliant on good bagging technique to ensure you have no bridges.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant