By carbon man - 12/22/2017 9:46:18 AM
Hi can I have some tips on how to get carbon to sit in tight and straight without using spray glue?
|
By Warren (Staff) - 1/2/2018 9:14:45 AM
You can use tape on the fabric edge to help a bit, but without any spray tack, you are reliant on good bagging technique to ensure you have no bridges.
|
|