Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
I would still go from one side to the other. As well as the usual U shape of spiral, I would add a couple of short lengths to ensure resin gets down to the bottom of the mould where the roof is.. Put the vacuum port on the sill.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|